13. Boriding kinetics of Fe2B layers formed on AISI 1045 steel / J. Zuno-Silva, M. Ortiz-
Domínguez, M. Keddam, M. Elias-Espinosa, O. Damián-Mejía, E. Cardoso-Legorreta, M. Abreu-
Quijano // Journal of Mining and Metallurgy, Section B: Metallurgy. – 2014. – Vol. 50, iss. 2. – P.
101–107.
14. Boriding of Equiatomic Fe-Mn Binary Alloy / A. Calika, Y. Gencerb, M. Tarakcib, K.O.
Gunduzb, A.E. Gulecb // Acta Physica Polonica A. – 2013. – Vol. 123, N 2. – P. 449–452. – doi:
10.12693/APhysPolA.123.449.
15.
Gunes I., Kayali Yu., Ulu S.
Investigation of surface properties and wear resistance of
borided steels with different B4C mixtures // Indian Journal of Engineering & Material Sciences. –
2012. – Vol. 19 (6). – P. 397–402.
16.
Campos-Silva I.
The boriding process: growth kinetics and mechanical characterization
of boride layers // JESTECH. – 2012. – Vol. 15 (2). – P. 53–61.
17.
Milinović A., Krumes D., Marković R.
An investigation of boride layers growth kinetics
on carbon steels // Technical Gazette. – 2012. – Vol. 19 (1). – P. 27–31.
18.
Krzyminski H.
Process for boriding steel: patent US 3806374. – Publ. date 23.04.1974.
19.
Sutrisno S.B., Hikam M.
Surface hardening of St41 low carbon steel by using the
boronizing powder and pressured-heating technique // Research Journal of Material Sciences. –
2013. – Vol. 1 (10). – P. 1–5.
20.
Gunes I., Ozcatal M.
Diffusion kinetics and characterization of borided AISI H10 steel //
Materials and Technology. – 2015. – Vol. 49 (5). – P. 759–763.
CHANGE THE SIZE AND SURFACE ROUGHNESS SAMPLES OF STEEL St3
IN DIFFUSION SATURATION OF BORON, CHROMIUM AND TITANIUM
Guriev A.M.,
D.Sc.(Engineering), Professor, e-mail:
gurievam@mail.ruIvanov S.G.,
Ph.D. (Engineering), Engineer, e-mail:
serg225582@mail.ruGuriev M.A.,
Ph.D. (Engineering), Doctoral candidate, e-mail:
gurievma@mail.ruSobachkin A.V.,
Ph.D. (Engineering), Senior researcher, e-mail:
pr_mech@mail.ruIvanova T.G.,
Ph.D. student, e-mail:
tatiana-8989@mail.ruI.I. Polzunov Altai State Technical University, 46 Lenina avenue, Barnaul, Altai region, 656038,
Russian Federation
Abstract
The evolution of the studied sample sizes and masses of steel St3 depending on deposition
process parameters of multicomponent of diffusion coatings based on boron, chromium and
titanium. Growth steel specimen dimensions substantially independent of the composition of the
saturating medium and the method saturation. The size increase an average of 0.12 mm for every
100 microns thickness of the diffusion layer. The surface roughness of the samples of steel St3
depends on the composition of saturating medium and the saturation method.
Keywords
boron, chromium, titanium, boriding, steel, coating, diffusion